Very... VERY interesting... Rust Removal
Moderators: The Dark Side of Will, Series8217
Very... VERY interesting... Rust Removal
I came across a blurb of a bunch of englishmen doing a rapid-resto on a sick friend's lotus.
APPARANTLY, one of them dragged in a plastic 50gal drum, a couple of large iron anodes, and they were using this to strip rust off of steel/iron parts.
Now, I know the theory here, and as luck would have it, I DO in fact have access to a 50gal plastic drum.
Thing is, my grade-9 chemistry memory is failing, and I don't really know how I'd proceed given some half-remembered assumptions and concerns...
1) AC current is useless for this, since the ions would just be jogging back and forth, right?
2) How the hell would I make this at all "safe." I've stood in a puddle of electrified water when our garage flooded. It's not an experience I wish to repeat.
3) What voltage/amperage requirements would I need?
4) I know the anode MUST be iron (replacing FeO(x)- ions with Fe- ions, right?), but I'll be damned if I know what other element the other would need to be so that it doesn't produce anything too toxic or flammable... Zinc maybe?
5) What's to stop me from adding some salts to the mix and plating said parts with a similar setup for increased corrosion resistance?
APPARANTLY, one of them dragged in a plastic 50gal drum, a couple of large iron anodes, and they were using this to strip rust off of steel/iron parts.
Now, I know the theory here, and as luck would have it, I DO in fact have access to a 50gal plastic drum.
Thing is, my grade-9 chemistry memory is failing, and I don't really know how I'd proceed given some half-remembered assumptions and concerns...
1) AC current is useless for this, since the ions would just be jogging back and forth, right?
2) How the hell would I make this at all "safe." I've stood in a puddle of electrified water when our garage flooded. It's not an experience I wish to repeat.
3) What voltage/amperage requirements would I need?
4) I know the anode MUST be iron (replacing FeO(x)- ions with Fe- ions, right?), but I'll be damned if I know what other element the other would need to be so that it doesn't produce anything too toxic or flammable... Zinc maybe?
5) What's to stop me from adding some salts to the mix and plating said parts with a similar setup for increased corrosion resistance?
"Oh, this is too good. She thinks you're a servant... Cause you're black! This is greatest moment in my miserable life... Sooo-ey! I LOVE RACISM!"
they did that on an episode of horsepower TV on spike tv. http://www.powerblocktv.com/sites/horsepower/
baking soda and a battery charger with a 2 amp slow charge should work.
baking soda and a battery charger with a 2 amp slow charge should work.
2002 Camaro SS
1986 Fiero GT 3800SC 4T65E-HD
slp 1.8 rockers, slp headers, northstar throttle body, Z06 MAF,3.3" pulley,160 drilled stat,
12" Corvette brakes
1.81 60' 13.004 @102
new best 1.939 60' 12.909 @ 104.50
1986 Fiero GT 3800SC 4T65E-HD
slp 1.8 rockers, slp headers, northstar throttle body, Z06 MAF,3.3" pulley,160 drilled stat,
12" Corvette brakes
1.81 60' 13.004 @102
new best 1.939 60' 12.909 @ 104.50
-
- Posts: 70
- Joined: Sat Jun 11, 2005 12:21 am
A pressure washer and some acid used at the swimming pool will do the trick. Wash the rusty part to get all the oil/grease off, put the acid in a sprayer and soak the rust, wait a bit and pressure wash it off. Whatever rust is left, hit it with the acid again. When it has been rinsed, spray it down with some rust treatment (Extend, Rust Mort), prep and paint. Be prepared for some serious stink.
-
- Posts: 65
- Joined: Wed Jun 01, 2005 11:46 pm
- Location: Lexington, KY
- Series8217
- 1988 Fiero Track Car
- Posts: 6078
- Joined: Thu Jun 02, 2005 9:47 pm
- Location: Los Angeles, CA
I'm not worried about disposal.
I'm more interested in figuring out what metal would be best to plate parts in to slow down corrosion and/or provide a good solid base for paint.
I know nickel is popular...
I think I'm going to try nickel-plating the dogbone I made for my swap using nickel-chloride and a battery charger. It's looking a little haggard from the moisture, since I never got round to painting it. :salute:
I'll see how that works, and maybe build myself a bigger rectifier...
Although from what I gather in my readings, the slower the deposition, the stronger the coating.
Looks like I'll need two baths.
Step 1) The first will be to "electropolish" the item, which puts the piece on the anode in a Sodium bicarb bath, with a This will strip any rust oxides, as well as strip off a few molecules of iron, leaving a bright, shiny (and rust free finish)
Step 2) Rinse with deionized water, hook up cathode, dump into solution of Nickel Chloride.
Step 3) Soak for one 15m on, 15m off for about 24 hours (w/ help of timer)
Step 4) ???
Step 5) Profit
I'm more interested in figuring out what metal would be best to plate parts in to slow down corrosion and/or provide a good solid base for paint.
I know nickel is popular...
I think I'm going to try nickel-plating the dogbone I made for my swap using nickel-chloride and a battery charger. It's looking a little haggard from the moisture, since I never got round to painting it. :salute:
I'll see how that works, and maybe build myself a bigger rectifier...
Although from what I gather in my readings, the slower the deposition, the stronger the coating.
Looks like I'll need two baths.
Step 1) The first will be to "electropolish" the item, which puts the piece on the anode in a Sodium bicarb bath, with a This will strip any rust oxides, as well as strip off a few molecules of iron, leaving a bright, shiny (and rust free finish)
Step 2) Rinse with deionized water, hook up cathode, dump into solution of Nickel Chloride.
Step 3) Soak for one 15m on, 15m off for about 24 hours (w/ help of timer)
Step 4) ???
Step 5) Profit
"Oh, this is too good. She thinks you're a servant... Cause you're black! This is greatest moment in my miserable life... Sooo-ey! I LOVE RACISM!"
- Series8217
- 1988 Fiero Track Car
- Posts: 6078
- Joined: Thu Jun 02, 2005 9:47 pm
- Location: Los Angeles, CA
Ass :la:
I didn't mean I'd dump it in my neighbor's pond...
I work for a sustainability company, I've got LOTS of inroads to toxic waste processing facilities.
Besides, the water's the easy part; I'd just throw the block-heater element I have into it and let it perc off the water, leaving the nasty heavy metals in powder form that I can scrape up and either keep for later or dispose safely.
I didn't mean I'd dump it in my neighbor's pond...
I work for a sustainability company, I've got LOTS of inroads to toxic waste processing facilities.
Besides, the water's the easy part; I'd just throw the block-heater element I have into it and let it perc off the water, leaving the nasty heavy metals in powder form that I can scrape up and either keep for later or dispose safely.
"Oh, this is too good. She thinks you're a servant... Cause you're black! This is greatest moment in my miserable life... Sooo-ey! I LOVE RACISM!"
Sounds like a ton of work. My buddy joe turned me on to a product called POR15, this stuff is great. It adheres to rust better than to a clean surface. It's black out of the can, but paintable. And my buddy Sean used it on his CJ a couple months back, accidentally let some dry where he didn't want it- it took 30 minutes with a palm sander and 60 grit paper to get it back down to bare metal.
I wasn't talking about frame/body components. My car is a coast-car, so it's got very little of either.
The things that I want cleaned/fixed are items that are visible, and that would look better with some sort of corrosion resistant finish on them.
For example, the dogbone I made looked nice when I made it and cleaned it... But bare mild steel doesn't look so hot when it flash-rusts.
Other items would be assorted exposed bolts/studs, a few brackets, etc etc.
I just need to find a good source for Nickel sulfate in the city. I know it's cheap, and nickle-plating looks awesome...
Just that there isn't enough in a chemistry set to play with
The things that I want cleaned/fixed are items that are visible, and that would look better with some sort of corrosion resistant finish on them.
For example, the dogbone I made looked nice when I made it and cleaned it... But bare mild steel doesn't look so hot when it flash-rusts.
Other items would be assorted exposed bolts/studs, a few brackets, etc etc.
I just need to find a good source for Nickel sulfate in the city. I know it's cheap, and nickle-plating looks awesome...
Just that there isn't enough in a chemistry set to play with

"Oh, this is too good. She thinks you're a servant... Cause you're black! This is greatest moment in my miserable life... Sooo-ey! I LOVE RACISM!"
-
- Peer Mediator
- Posts: 15750
- Joined: Wed Nov 24, 2004 11:13 pm
- Location: In the darkness, where fear and knowing are one
- Contact:
Dude... Brushed nickel SO much nicer looking than SS. :salute:
Found a source, and at like $25 for a 5kg bag, too...
Althought I'm wondering if I should plate in copper first, then nickel (like professional chroming). Copper Sulfate is REALLY easy to find. Pesticides are rapidly going the way of Gun Control, so there's a brisk trade in Copper Sulfate for bio-shocking ponds/algae infested pools.
I'd *almost* consider trying to make my own chrome, except that any and all of the chromium salts score pretty high on the "you don't want to fuck with" scale.
Nickel Sulfate is bad enough--it's a pretty ripe carcinogen.
Oops, and I almost forgot a bit of highschool chemistry; I need an acid solution strong enough to dissolve nickel at the same rate as deposition. Fortunately, there's plenty of nickel in our Canadian Nickels (plated--thick-- at 25% by mass, as long as I have any minted before 2002--which I do; a whole sock drawer of 'em...)
Found a source, and at like $25 for a 5kg bag, too...
Althought I'm wondering if I should plate in copper first, then nickel (like professional chroming). Copper Sulfate is REALLY easy to find. Pesticides are rapidly going the way of Gun Control, so there's a brisk trade in Copper Sulfate for bio-shocking ponds/algae infested pools.
I'd *almost* consider trying to make my own chrome, except that any and all of the chromium salts score pretty high on the "you don't want to fuck with" scale.
Nickel Sulfate is bad enough--it's a pretty ripe carcinogen.
Oops, and I almost forgot a bit of highschool chemistry; I need an acid solution strong enough to dissolve nickel at the same rate as deposition. Fortunately, there's plenty of nickel in our Canadian Nickels (plated--thick-- at 25% by mass, as long as I have any minted before 2002--which I do; a whole sock drawer of 'em...)
"Oh, this is too good. She thinks you're a servant... Cause you're black! This is greatest moment in my miserable life... Sooo-ey! I LOVE RACISM!"
-
- Posts: 290
- Joined: Wed Aug 16, 2006 12:14 pm
- Location: Alberta
Re: Very... VERY interesting... Rust Removal
Um, the other element is the part you're removing rust from... The electrolyte is the only real factor if you're concerned about toxic / flammable vapours.Mach10 wrote: 4) I know the anode MUST be iron (replacing FeO(x)- ions with Fe- ions, right?), but I'll be damned if I know what other element the other would need to be so that it doesn't produce anything too toxic or flammable... Zinc maybe?
Yeah, that's the gist of it.Mach10 wrote: 5) What's to stop me from adding some salts to the mix and plating said parts with a similar setup for increased corrosion resistance?
Why would you eat bad ice cream?